LOTEK 4200 (Ethylene Acrylic Acid Zinc  IONOMER)

Key features

Recommended processing conditions and resin handling

IOTEK 4200 is a zinc ionomer, which offers :

- good sealability, high hot tack and seal 
   through contamination
- good adhesion on paper, aluminium,   
   poly-amide and  polyethylene.
- excellent draw down/neck-in balance in 
   extrusion coating.
- film of high impact strength and puncture 
   resistance
- low odor

It is primarily used for extrusion coating and film coextrusion applications.

Processing conditions:
Extrusion coating : 275-300°C.
Blown film : 180-220°C.

Blown film : 180-230°C.
Higher processing temperatures favor the optical properties.

Warning:

To minimize corrosion risk, all exposed metal surfaces in the extruder and die should be made from corrosion resistant metals or nickel/chrome plated. 

Iotek 4200 should be fed into the extruder after LDPE of a similar or higher melt index. Machines should always be completely purged with LDPE or a suitable cleaning compound before shutdown.

Cation containing polymers pick up moisture from the atmosphere if exposed for prolonged periods. It is therefore recommended to re-seal  tightly the package after each production run molding.

Typical values

 General properties Test Method(based on) Unit Typical Value
Melt index D 1238 g/10 min 3
Density D 1928 / 1505 g/cm 3 0.946
Melting point (DSC) D 3418 °C 94
Crystallization point (DSC) D 3418  °C 73
Vicat Softening Point D 1525 °C 73

Plaque properties

Test Method(based on) Unit Typical Value
Tensile strength at break D 638 MPa 24
Yield strength D 638 MPa 9
Elongation at break D 638 % 600
1 % Secant Modulus D 638 MPa 120
Abrasion resistance (weight loss) D 1242 mg 33

Film properties

          
Tensile Strength at Break MD / TD D 882 MPa 29 / 24
Yield Strength MD / TD D 882 MPa 12 / 10
Elongation at break MD / TD D 882 % 350 / 380
1 % Secant Modulus  MD / TD D 638 MPa 130 / 140
Haze   D 1003 % 4
Clarity   D 1746 % 9
Dart Drop Impact (A/Face)    D 1709 g/µm 12
Elmendorf Tear Strength MD / TD D 1922 g/µm 5 / 8.5